Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Can Nansulate® EPX be applied at 2″ thick to achieve minimum heat loss on hot water tanks?

0
Posted

Can Nansulate® EPX be applied at 2″ thick to achieve minimum heat loss on hot water tanks?

0

With any insulation, the outside and inside temperatures will eventually reach an equilibrium unless there is an additional heating source, however Nansuate® EPX can help them retain the heat as long as possible. Yes, it can be built up to a 2″ or more thickness if desired.