Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Can Pressure Sequence Hydroforming (PSH) form a tight cross section corner?

0
Posted

Can Pressure Sequence Hydroforming (PSH) form a tight cross section corner?

0

A- Yes, the PSH design guide recommends a target value of 4 times material thickness for the outside corner radius of a cross section. However local cross sections have been formed with corners as small as 2 times the material thickness without using high pressure and no material thinning.