Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

How do extremes of humidity and temperatures affect Slavich Holography materials?

0
Posted

How do extremes of humidity and temperatures affect Slavich Holography materials?

0

Very high humidity (>85%) should always be avoided as they will degrade the lifetime rapidly. Medium to low humidity are acceptable with low humidity being optimal. Temperatures above 80 Degrees C lead to the PFG-03 material becoming sensitive to the polarization of light. Also exposure to such high temperatures will produce a gradual decrease in sensitivity. Short exposures of all materials to temperatures up to 50 Degrees C will not affect performance or greatly reduce the lifetime. Transport of the materials through hot countries is generally not a problem. • Will the PFG-03M plates work with a HeCd laser of 40mW? The green (514nm) sensitivity is about 5x worse than the red (633nm) and 442nm is around 1.5 x better than the green. • What must my PFG03M plate look like after developing? This depends on the developer but usually this must be a light to deep brown. Initially the plates should be transparent/blue. Note that for VRP/M/PFG-01 the plates before development are transparent a

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.