Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

What is the minimum degree of roughness (texturing) a textured liner should have?

0
Posted

What is the minimum degree of roughness (texturing) a textured liner should have?

0

The minimum industry standard specification GRI GM13 and GRI GM17, require a minimum Asperity Height of 10 mils for textured HDPE and textured LLDPE geomembranes. • What are the temperatures for material that can be contained by Poly-Flex liners? Poly-Flex geomembranes are thermoplastic materials, hence their physical properties are temperature dependent. The material becomes softer and more flexible at higher temperatures and stiffer and stronger at lower temperatures. We specify maximum use temperatures of 160° F for HDPE and 140° F for LLDPE liners. • What is the cold temperature resistance of Poly-Flex liners? Poly-Flex liners pass the low temperature brittleness test at -70° C (-94° F) according to the ASTM D 746. • Why do Poly-Flex liners have wrinkles? Polyethylene liners expand and contract as the sheet temperature changes. This thermal expansion/contraction will cause the liner to grow or shrink with variance in temperature. • Are Poly-Flex liners available in any other colors

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.