Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Why do I see air bubbles, wrinkles, ripples, sharp corners and temperature shrinking problems with Eco Shrink FIlm?

0
Posted

Why do I see air bubbles, wrinkles, ripples, sharp corners and temperature shrinking problems with Eco Shrink FIlm?

0

These problems typically occur when Eco Shrink Film is ran through a shrink film machine as a single sheet. This shrink film is centerfolded, which means there are two layers to the film. Ensure you have the product positioned between the centerfolded film to avoid these common problems. 30. What temperature should I run Eco Shrink Film at on my automated machine? Return to Top Eco Shrink Film should be ran at 180-240 degrees Fahrenheit. Start your machine at the low temperature and increase up to 240 degrees or until you achieve a satisfactory seal. Running the film too hot can cause “angel hairs” due to the film melting instead of sealing. Eco Shrink Film may not run on high speed automated shrink sealing systems. ClearBags recommends you sample and test before ordering in volume. 31. Is Moab paper compatible with dye-based inks? Return to Top Moab papers are compatible but not optimized for dye-based inks Entrada and other cotton papers will show little visible difference, but micro

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.