Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

How Do You Make Fused Glass Cabochons?

0
Posted

How Do You Make Fused Glass Cabochons?

0

• Place the paper on the kiln shelf. Assemble your glass pieces with the glass cap placed evenly on top of the dichroic, with the dichroic layer facing up. • The clear cap needs to be larger than the base as the dichroic layer can sometimes seep out under the clear glass. • Ripple dichroic may require a larger cap as the clear glass will sink down into the ripples. • Set the temperature on the kiln to medium for about 15 minutes, if using a manual kiln. Bring up to 1500°F (815°C) per hour and hold for 10 minutes. If using a programmable kiln, ramp your temperature up to 1500°F per hour and hold for 10 minutes. Check that your cabochons have fully fused. If not, let the temperature return to 1500°F and hold for another 5 minutes. • The above instructions are for Bullseye glass. The firing details can be used for most cabochons which are less than 2 inches all around. • Once the glass has fully fused, turn the kiln off and open the door until the temperature reaches 1000°F (540°C). Close

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.