Important Notice: Our web hosting provider recently started charging us for additional visits, which was unexpected. In response, we're seeking donations. Depending on the situation, we may explore different monetization options for our Community and Expert Contributors. It's crucial to provide more returns for their expertise and offer more Expert Validated Answers or AI Validated Answers. Learn more about our hosting issue here.

Can the chitin beads be regenerated?

beads chitin regenerated
0
Posted

Can the chitin beads be regenerated?

0

The chitin beads can be regenerated at least 5 times. After stripping the chitin column with 3 volumes of 0.3 M NaOH (Stripping solution). Allow the beads to soak for 30 minutes, wash the resin with additional 7 column volumes of 0.3 M NaOH. Then wash the resin with 20 bed volumes of water followed by 5 column volumes of Column Buffer. For long term storage, add 0.02% sodium azide to the Column Buffer. The beads should be stored at 4°C. Temporary storage at -20°C will not affect the binding capacity.

Related Questions

What is your question?

*Sadly, we had to bring back ads too. Hopefully more targeted.