We are interested in Sulfide Stress Corrosion cracking testing (NACE TM0177) at 24 deg C on a 13mm bar stock?
At TCR Engineering Services, we can definitely undertake the NACE TM0177 testing at 24deg C at our laboratory in Navi Mumbai, India. We have been routinely undertaking this test for a large number of customers all over the world. We will require a 200mm long sample (8 inch long) of your 13mm bar stock. In our laboratory we can run upto 10 SSCC tests in parallel. For your samples we can accommodate 5 tests in parallel. We will begin the test within 3 days of receipt of the sample. The cost of the test will be US$600 for 720 hours of SSCC test as per NACE TM0177. A mandatory 12.24% service tax will be extra. Payment can be made via Bank wire transfer or via Credit Card (using Paypal). You will have to ship the samples to: TCR Engineering Services Pvt. Ltd. ATTN: Sample Receipt 35 Pragati Industrial Estate, N.